Density of some common liquids:

Liquids - Densities
LiquidTemperature
- t -
(oC)

Density
- ρ -
(kg/m3)



Acetaldehyde 18 783
Acetic Acid 25 1049
Acetone 25 784.6
Acetonitrile 20 783
Acrolein 20 840
Acrolonitrile 25 801
Alcohol, ethyl (ethanol) 25 785.1
Alcohol, methyl (methanol) 25 786.5
Alcohol, propyl 25 800.0
Almond kernel oil 25 910
Alyllamine 20 758
Ammonia (aqua) 25 823.5
Aniline 25 1019
Anisole 20 994
Antifreeze mixtures (solutions)
Apricot kernel oil 25 910
Argan seed oil 20 912
Automobile oils 15 880 - 940
Avacado pulp oil 25 912
Babassu palm oil 25 914
Beef tallow (land animals) 25 902
Beer (varies) 10 1010
Benzaldehyde 25 1040
Benzene 25 873.8
Benzil 15 1230
Blackcurrant oil 20 923
Borneo tallow 100 855
Brine 15 1230
Bromine 25 3120
Butanal 20 802
Butterfat (land animals) 15 934
Butyric Acid 20 959
Butane 25 599
2,3-Butandione 18 981
2-Butanone 25 800
n-Butyl Acetate 20 880
n-Butyl Alcohol (Butanol) 20 810
n-Butylhloride 20 886
Cameline oil 15 924
Canola rapeseed oil 20 915
Caproic acid 25 921
Carbolic acid (phenol) 15 956
Carbon disulfide 25 1261
Carbon tetrachloride 25 1584
Carene 25 857
Cashew nut oil 15 914
Castor oil 25 952
Cherry kernel oil 25 918
Chicken fat 15 918
Chinese vegable tallow 25 887
Chloride 25 1560
Chlorobenzene 20 1106
Chloroform 20 1489
Chloroform 25 1465
Citric acid, 50% aqueous solution 15 1220
Cocoa butter 25 974
Coconut oil 40 930
Cod liver oil 15 924
Cohune nut oil 25 914
Corn oil 20 919
Corriander seed oil 25 908
Cotton seed oil 20 920
Crambe oil 25 906
Cresol 25 1024
Creosote 15 1067
Crude oil, 48o API 60 oF (15.6 oC) 790
Crude oil, 40o API 60 oF (15.6 oC) 825
Crude oil, 35.6o API 60 oF (15.6 oC) 847
Crude oil, 32.6o API 60 oF (15.6 oC) 862
Crude oil, California 60 oF (15.6 oC) 915
Crude oil, Mexican 60 oF (15.6 oC) 973
Crude oil, Texas 60 oF (15.6 oC) 873
Cumene 25 860
Cyclohexane 20 779
Cyclopentane 20 745
Decane 25 726.3
Diesel fuel oil 20 to 60 15 820 - 950
Diethanolamine 20 1097
Diethyl ether 20 714
o-Dichlorobenzene 20 1306
Dichloromethane 20 1326
Diethyl ether 20 714
Diethylene glycol 15 1120
Diethylene glycol diethyl ether 20 906
Dichloromethane 20 1326
Diisopropyl ether 25 719
Dimethyl acetamide 20 942
N,N-Dimethylformamide 20 949
Dimethyl sulfate 20 1332
Dimethyl sulfide 20 848
Dimethyl sulfoxide 20 1100
Dodecane 25 754.6
Ethane -89 570
Ethanol 20 790
Ethanol 95% 20 810
Ether 25 713.5
Ethylamine 16 681
Ethyl Acetate 20 901
Ethyl Alcohol (Ethanol, pure alcohol, grain alcohol or drinking alcohol) 20 789
Ethyl chloride 20 900
Ethyl Ether 20 713
Ethylene Dichloride 20 1253
Ethylene glycol 25 1097
Euphorbia lagascae seed oil 25 952
Trichlorofluoromethane refrigerant R-11 25 1476
Dichlorodifluoromethane refrigerant R-12 25 1311
Chlorodifluoromethane refrigerant R-22 25 1194
Formaldehyde 45 812
Formic acid 10% concentration 20 1025
Formic acid 80% concentration 20 1221
Fuel oil 60 oF (15.6 oC) 890
Furan 25 1416
Furforal 25 1155
Gasoline, natural 60 oF (15.6 oC) 711
Gasoline, Vehicle 60 oF (15.6 oC) 737
Gas oils 60 oF (15.6 oC) 890
Glucose 60 oF (15.6 oC) 1350 - 1440
Glycerine (glycerol 95%, water 5%) 25 1249
Glycerol 25 1261
Grape seed oil 20 923
Hazelnut oil 25 909
Heating oil 20 920
Hempseed oil 25 921
Heptane 25 679.5
Herring oil 20 914
Hexane 25 654.8
Hexanol 25 811
Hexene 25 671
Hexylamine 20 766
Hydrazine 25 795
Illipe mowrah butter 100 862
Ionene 25 932
Isobutyl Alcohol 20 802
Iso-Octane 20 692
Isopropyl Alcohol 20 785
Isopropylbenzene hydroperoxide 20 1030
Isopropyl Myristate 20 853
Kapok seed oil 15 926
Kerosene (paraffin) 60 oF (15.6 oC) 820.1
Linolenic Acid 25 897
Linseed oil 25 924
Lubricating oil 20 910
Machine oil 20 910
Mango seed oil 15 912
Menhaden oil 15 920
Mercury 13590
Methane -164 465
Methanol 20 791
Methylamine 25 656
Methyl chloride 20 990
Methyl Isoamyl Ketone 20 888
Methyl Isobutyl Ketone 20 801
Methyl n-Propyl Ketone 20 808
Methyl t-Butyl Ether 20 741
N-Methylpyrrolidone 20 1030
Methyl Ethyl Ketone 20 805
Milk 15 1020 - 1050
Moringa peregrina seed oil 24 903
Mustard seed oil 20 913
Mutton tallow 15 946
Naphtha 15 665
Naphtha, wood 25 960
Napthalene 25 820
Neem oil 30 912
Niger seed oil 15 924
Nitric acid 0 1560
Oat been oil 25 904
Oat oil 25 917
Ocimene 25 798
Octane 15 698.6
Oil of resin 20 940
Oil of turpentine 20 870
Oil, lubricating 20 900
Oiticica oil 20 972
Olive oil 20 911
Oxygen (liquid) -183 1140
Palm kernel oil 15 922
Palm oil 15 914
Palm olein 40 910
Palm stearin 60 884
Paraldehyde 20 994
Paraffin oil 800
Palmitic Acid 25 851
Peanut oil 20 914
Pentane 20 626
Pentane 25 625
Perchlor ethylene 20 1620
Perilla oil 25 924
Petroleum ether 20 640
Petrol, natural 60 oF (15.6 oC) 711
Petrol, Vehicle 60 oF (15.6 oC) 737
Phenol (carbolic acid) 25 1072
Phosgene 0 1378
Phytadiene 25 823
Phulwara butter 100 862
Pinene 25 857
Pine nut oil 15 919
Poppy seed oil 25 916
Pork lard 20 898
Propanal 25 866
Propane -40 493.5
Propane, R-290 25 494
Propanol 25 804
Propylamine 20 717
Propylenearbonate 20 1201
Propylene 25 514.4
Propylene glycol 25 1036
Pyridine 25 979
Pyrrole 25 966
Rapeseed oil 20 920
Resorcinol 25 1269
Rice bran oil 25 916
Rosin oil 15 980
Salmon oil 15 924
Sardine oil 25 915
Sea water 25 1025
Seaflower seed oil 15 924
Shark liver oil 25 917
Sheanut butter 100 863
Silane 25 718
Silicone oil 25 965 - 980
Sodium Hydroxide (caustic soda) 15 1250
Sorbaldehyde 25 895
Soybean oil 20 920
Stearic Acid 25 891
Stillinga seed kernel oil 25 937
Sulfur dichloride 1620
Sulfuric Acid 95% concentration 20 1839
Sulfurus acid -20 1490
Sulfuryl chloride 1680
Sugar solution 68 brix 15 1338
Sunflower seed oil 20 919
Styrene 25 903
Tall oil 25 969
Tar 20 1200
Terpinene 25 847
Tetrahydrofuran 20 888
Toluene 20 867
Transformer oil 20 880
Trichlorethylene 20 1470
Triethylamine 20 728
Trifluoroacetic Acid 20 1489
Tung oil 25 912
Turpentine oil 25 860
Ucuhuba butter oil 100 870
Vernonia seed oil 30 901
Walnut oil 25 921
Water, heavy 11.6 1105
Water - pure 4 1000
Water - sea 77 oF (25 oC) 1022
Whale oil 15 925
Wheatgerm oil 25 926
o-Xylene 20 880
m-Xylene 20 864
p-Xylene 20 861
  • 1 kg/m3 = 0.001 g/cm3 = 0.0005780 oz/in3 = 0.16036 oz/gal (Imperial) = 0.1335 oz/gal (U.S.) = 0.0624 lb/ft3 = 0.000036127 lb/in3 = 1.6856 lb/yd3 = 0.010022 lb/gal (Imperial) = 0.008345 lb/gal (U.S) = 0.0007525 ton/yd3

Note that even if pounds per cubic foot is often used as a measure of density in the U.S., pounds are really a measure of force, not mass. Slugs are the correct measure of mass. You can divide pounds per cubic foot by 32.2 for a rough value in slugs.

Sponsored Links

Related Topics

Densities

Densities of solids, liquids and gases. Definitions and convertion calculators.

Fluid Flow and Pressure Loss in Pipes and Tubes

Fluid flow and pressure loss in pipe lines. Water and sewer systems. Steel pipes, pvc pipes, copper tubes and more.

Material Properties

Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Alcohols and Carboxylic Acids - Physical Data

Molweight, melting and boiling point, density, pKa-values, as well as number of carbon and hydrogen atoms in molecules are given for 150 different alcohols and acids.

API Gravity: Definition, Calculation, and Converter

API expresses the gravity or density of liquid petroleum products. Online API to Specific Gravity calculator.

Crude Oil - Density vs. Temperature

Variations in crude oil density are shown as function of temperatur, together with volume correction factors.

Densities of Aqueous Solutions of Inorganic Chlorides

Changes in density of aqueous solutions with changes in concentration at 20°C. Density of inorganic chlorides in water is plotted as function of wt%, mol/kg water and mol/l solution.

Densities of Aqueous Solutions of Inorganic Potassium Salts

Changes in density of aqueous solutions with changes in concentration at 20°C. Density of potassium salts in water is plotted as function of wt%, mol/kg water and mol/l solution.

Densities of Aqueous Solutions of Inorganic Sodium Salts

Changes in density of aqueous solutions with changes in concentration at 20°C. Density of inorganic sodium salts in water is plotted as function of wt%, mol/kg water and mol/l solution.

Densities of Aqueous Solutions of Organic Acids

Changes in density of aqueous solutions with changes in concentration at 20°C. Density of acetic acid, citric acid, formic acid, D-lactic acid, oxalic acid and trichloroacetic acid in water is plotted as function of wt%, mol/kg water and mol/l solution.

Density Converter

Online density converter with commonly used units.

Density of Aqueous Solutions of Organic Substances as Sugars and Alcohols

Changes in density of aqueous solutions with changes in concentration at 20°C. Density of some sugars, alcohols and other organic substances in water is plotted as function of wt%, mol/kg water and mol/l solution.

Density of Aqueous Solutions of some Inorganic Substances

Changes in density of aqueous solutions with changes in concentration at 20°C. Density of inorganic substances in water is plotted as function of wt%, mol/kg water and mol/l solution.

Ethanol Water Mixtures - Densities vs. Temperature

Density of Ethyl Alcohol aqueous solutions.

Fuel Oils - Densities vs. Temperature

Variations in fuel oils density as function of temperatur, together with volume correction factors.

Hydrocarbons - Physical Data

Molweight, melting and boiling point, density, flash point and autoignition temperature, as well as number of carbon and hydrogen atoms in each molecule for 200 different hydrocarbons.

Hydrocarbons, Linear Alcohols and Acids - Densities

Density of hydrocarbons like alcohols and acids as function of carbon number at 20°C / 68°.

ISO Grade Oils - Viscosities and Densities

Viscosities and densities of ISO - and equivalent SAE grade oils.

Jet Fuel - Density vs. Temperature

Variations in jet fuel density as function of temperatur, together with volume correction factors.

Liquids - Densities vs. Pressure and Temperature Change

Densities and specific volume of liquids vs. pressure and temperature change.

Liquids - Specific Gravities

Specific gravities of liquids like alcohol, oils, benzene, water and many more.

Liquids and Gases - Boiling Points

Boiling temperatures for common liquids and gases - acetone, butane, propane and more.

Lubricating Oil - Densities vs. Temperature

Variations in lubricating oil density as function of temperatur, together with volume correction factors.

Mass vs Weight

Mass vs. weight - the Gravity Force.

Methanol - Thermophysical Properties vs. Temperature

Thermophysical properties of methanol.

Minerals - Densities

Densities of minerals.

Oil Fuels - Viscosities vs. Temperatures

Viscosities of fuel oils vs. temperature.

Oils - Melting points

Common oils from animals or plants and their melting points.

Organic Sulfur Compounds - Densities

Liquid density of different kinds of organic sulfur compounds with varying carbon number (20°C/68°F). Comparison of thiols, sulfides, disulfides and thiophenes.

Piping Elbows - Thrust Block Forces

Thrust block forces on pipe bends anchors due to liquid velocities and internal pressures - online resulting force calculator.

Propane - Vapor Pressure vs. Temperature

Vapor pressure vs. temperature.

Salinity of Water

Salinity - salt content - of fresh, brackish and sea water.

Solids - Densities

Densities of selected solids.

Specific Heat of Common Liquids and Fluids

Specific heats for some common liquids and fluids - acetone, oil, paraffin, water and many more.

Sulfuric Acid - Density

Density of sulfuric acid at various temperatures and concentrations.

Water Density, Specific Weight and Thermal Expansion Coefficients - Temperature and Pressure Dependence

Data on the density and specific weight of water across various temperatures and pressures. Useful for engineering, fluid dynamics, and HVAC calculations.

Water Thermal Properties – Density, Heat Capacity, and Conductivity

Thermal properties of water, including density, specific heat capacity, thermal conductivity, and thermal expansion at different temperatures.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.