Stainless Steel - Comparing International Standards

Sponsored Links

For full table - rotate the screen!

Stainless Steel - Comparing International Standards
USAFranceGermanyGermanyItalyJapanRussiaSpainSwedenUKEuropean Union
AISIAFNORDIN 17006W.N. 17007UNIJISGOSTUNESISBSIEURONORM
201 1) SUS 201
301 1) Z 12 CN 17-07 X 12 CrNi 17 7 1.4310 X 12 CrNi 1707 SUS 301 X 12 CrNi 17-07 23 31 301S21 X 12 CrNi 17 7
302 1) Z 10 CN 18-09 X 5 CrNi 18 7 1.4319 X 10 CrNi 1809 SUS 302 12KH18N9 X 10 CrNi 18-09 23 31 302S25 X 10 CrNi 18 9
303 1) Z 10 CNF 18-09 X 10 CrNiS 18 9 1.4305 X 10 CrNiS 1809 SUS 303 X 10 CrNiS 18-09 23 46 303S21 X 10 CrNiS 18 9
303 Se 1) Z 10 CNF 18-09 X 10 CrNiS 1809 SUS 303 Se 12KH18N10E X 10 CrNiS 18-09 303S41
304 1) Z 6 CN 18-09 X 5 CrNi 18 10 X 5 CrNi 18 12 1.4301 1.4303 X 5 CrNi 1810 SUS 304 08KH18N10 06KH18N11 X 6 CrNi 19-10 23 32 304S15 304S16 X 6 CrNi 18 10
304 N 1) X 5 CrNiN 1810 SUS 304N1
304 H 1) X 8 CrNi 1910 SUS F 304H X 6 CrNi 19-10
304 L 1) Z 2 CN 18-10 X 2 CrNi 18 11 1.4306 X 2 CrNi 1911 SUS 304L 03KH18N11 X 2 CrNi 19-10 23 52 304S11 X 3 CrNi 18 10
Z 2 CN 18-10-Az X 2 CrNiN 18 10 1.4311 X 2 CrNiN 1811 SUS 304LN 23 71
305 1) Z 8 CN 18-12 X 8 CrNi 1812 SUS 305 X 8 CrNi 18-12 23 33 305S19 X 8 CrNi 18 12
Z 6 CNU 18-10 SUS XM7 X 6 CrNiCu 18 10 4 Kd
309 1) Z 15 CN 24-13 X 15 CrNiS 20 12 1.4828 X 16 CrNi 2314 SUH 309 309S24 X 15 CrNi 23 13
309 S 1) X 6 CrNi 2314 SUS 309S 20KH23N18 X 6 CrNi 22 13
310 1) X 12 CrNi 25 21 1.4845 X 22 CrNi 2520 SUH 310 10KH23N18 310S24
310 S 1) Z 12 CN 25-20 X 12 CrNi 25 20 1.4842 X 5 CrNi 2520 SUS 310S 20KH25N20S2 23 61 X 6 CrNi 25 20
314 1) Z 12 CNS 25-20 X 15 CrNiSi 25 20 1.4841 X 16 CrNiSi 2520 X 15 CrNiSi 25 20
316 1) Z 6 CND 17-11 X 5 CrNiMo 17 12 2 1.4401 X 5 CrNiMo 1712 SUS 316 X 6 CrNiMo 17-12-03 23 47 316S31 X 6 CrNiMo 17 12 2
316 1) Z 6 CND 17-12 X 5 CrNiMo 17 13 3 1.4436 X 5 CrNiMo 1713 SUS 316 X 6 CrNiMo 17-12-03 23 43 316S33 X 6 CrNiMo 17 13 3
316 F 1) X 12 CrNiMoS 18 11 1.4427
316 N 1) SUS 316N
316 H 1) X 8 CrNiMo 1712 SUS F 316H X 5 CrNiMo 17-12
316 H 1) X 8 CrNiMo 1713 03KH17N14M2 X 6 CrNiMo 17-12-03
316 L 1) Z 2 CND 17-12 X 2 CrNiMo 17 13 2 1.4404 X 2 CrNiMo 1712 SUS 316L X 2 CrNiMo 17-12-03 23 48 316S11 X 3 CrNiMo 17 12 2
Z 2 CND 17-12-Az X 2 CrNiMoN 17 12 2 1.4406 X 2 CrNiMoN 1712 SUS 316LN 03KH16N15M3
316 L 1) Z 2 CND 17-13 X 2 CrNiMo 18 14 3 1.4435 X 2 CrNiMo 1713 X 2 CrNiMo 17-12-03 23 53 316S13 X 3 CrNiMo 17 13 3
Z 2 CND 17-13-Az X 2 CrNiMoN 17 13 3 1.4429 X 2 CrNiMoN 1713 08KH17N13M2T 10KH17N13M2T 23 75
Z6 CNDT 17-12 X 6 CrNiMoTi 17 12 2 1.4571 X 6 CrNiMoTi 1712 08KH17N13M2T 10KH17N13M2T X 6 CrNiMoTi 17-12-03 23 50 320S31 X 6 CrNiMoTi 17 12 2
X 10 CrNiMoTi 18 12 1.4573 X 6 CrNiMoTi 1713 08KH16N13M2B X 6 CrNiMoTi 17-12-03 320S33 X 6 CrNiMoTI 17 13 3
Z 6 CNDNb 17-12 X 6 CrNiMoNb 17 12 2 1.4580 X 6 CrNiMoNb 1712 09KH16N15M3B X 6 CrNiMoNb 17 12 2
X 10 CrNiMoNb 18 12 1.4583 X 6 CrNiMoNb 1713 X 6 CrNiMoNb 17 13 3
317 1) X 5 CrNiMo 1815 SUS 317 23 66 317S16
317 L 1) Z 2 CND 19-15 X 2 CrNiMo 18 16 4 1.4438 X 2 CrNiMo 1815 SUS 317L 23 67 317S12 X 3 CrNiMo 18 16 4
317 L 1) Z 2 CND 19-15 X 2 CrNiMo 18 16 4 1.4438 X 2 CrNiMo 1816 SUS 317L 23 67 317S12 X 3 CrNiMo 18 16 4
330 1) Z 12NCS 35-16 X 12 NiCrSi 36 16 1.4864 SUH 330 08KH18N10T
321 1) Z 6 CNT 18-10 X 6 CrNiTi 18 10 X 12 CrNiTi 18 9 1.4541 1.4878 X 6 CrNiTi 1811 SUS 321 12KH18N10T X 6 CrNiTi 18-11 23 37 321S31 X 6 CrNiTi 18 10
321 H 1) X 8 CrNiTi 1811 SUS 321H X 7 CrNiTi 18-11 321S20
329 1) X 8 CrNiMo 27 5 1.4460 SUS 329J1 08KH18N12B 23 24
347 1) Z 6 CNNb 18-10 X 6 CrNiNb 18 10 1.4550 X 6 CrNiNb 1811 SUS 347 X 6 CrNiNb 18-11 23 38 347S31 X 6 CrNiNb 18 10
347 H 1) X 8 CrNiNb 1811 SUS F 347H X 7 CrNiNb 18-11
904L 1) Z 12 CNDV 12-02 1.4939
X 20 CrNiSi 25 4 1.4821
UNS31803 2) X 2 CrNiMoN 22 5 1.4462
UNS32760 2) Z 3 CND 25-06Az X 3 CrNiMoN 25 7 1.4501 12Kh13
403 3) Z 12 C 13 X 6 Cr 13 X 10 Cr 13 X 15 Cr 13 1.4000 1.4006 1.4024 X 12 Cr 13 SUS 403 X 6 Cr 13 23 02 403S17 X 10 Cr 13 X 12 Cr 13
405 3) Z 6 CA 13 X 6 CrAl 13 1.4002 X 6 CrAl 13 SUS 405 X 6 CrAl 13 405S17 X 6 CrAl 13
Z 8 CA 7 X 10 CrAl 7 1.4713 10Kh13SYu X 10 CrAl 7
X 10 CrAl 13 1.4724 X 10 CrAl 12 15Kh18SYu
X 10 CrAl 18 1.4742 X 10 CrSiAl 18
409 3) Z 6 CT 12 X 6 CrTi 12 1.4512 X 6 CrTi 12 SUH 409 409S19 X 5 CrTi 12
X 2 CrTi 12 12Kh13
410 3) Z 10 C 13 Z 12 C 13 X 6 Cr 13 X 10 Cr 13 X 15 Cr 13 1.4000 1.4006 1.4024 X 12 Cr 13 SUS 410 08Kh13 X 12 Cr 13 23 02 410S21 X 12 Cr 13
410 S 3) Z 6 C 13 X 6 Cr 13 1.4000 X 6 Cr 13 SUS 410S 23 01 403S17 X 6 Cr 13
414 3)

1) Austenitic grades

2) Ferritic austenitic grades, Duplex and Super Duplex

3) Ferritic grades

Sponsored Links

Related Topics

Piping Codes and Standards

Piping and tubes codes and standards - ASME, ANSI, ASTM, AGA, API, AWWA, BS, ISO, DIN and more.

Related Documents

AISI 310 Stainless Steel - Properties

Thermal diffusivity, specific heat capacity, density and thermal conductivity of stainless steel AISI 310 vs. temperature.

ASME/ANSI B36.10/19 - Carbon, Alloy and Stainless Steel Pipe - Dimensions

Pipe sizes, inside and outside diameters, wall thickness, schedules, moment of inertia, transverse area, weight of pipe filled with water - U.S. Customary Units.

ASTM A312 Stainless Steel Pipes - Bursting and Collapsing Pressures

Theoretic bursting and collapsing pressures for stainless steel pipes ASTM A312.

Carbon and Stainless Steel Flanges - ASME/ANSI Class 150

ASME/ANSI B16.5-1996 Pipe Flanges and Flanged Fittings - Class 150 Flanges - outside and inside diameters, bolt circles, numbers and diameters of bolts.

Composition of Steels

Typical composition of AISI steels.

Copper, Ductile Iron, Carbon Steel, Stainless Steel and Aluminum Piping Materials - Temperature Expansion

Thermal expansion of typical piping materials.

Metals and Alloys - Melting Temperatures

The melting temperatures for some common metals and alloys.

Piping Materials - Cost Ratios

Installing cost ratios for piping materials related to carbon steel pipes.

PVC, CPVC, Carbon Steel, Stainless Steel and Fiberglass Pipes - Thermal Expansion Diagrams

Thermal expansion of PVC, CPVC, Carbon and Stainless Steel and Fiberglass pipes.

Stainless Steel - Specific Heat and Thermal Conductivities vs. Temperatures

Specific heat and thermal conductivity of stainless steel vs. temperature

Stainless Steel Classifications

Stainless steels are commonly grouped into martensitic stainless steels, ferritic stainless steels, austenitic stainless steels, duplex (ferritic-austenitic) stainless steels, and precipitation-hardening stainless steels.

Stainless Steel Pipes - American vs. European Standards

American - US - vs. European - German, British (UK) and Swedish - stainless steel pipe standards.

Stainless Steel Pipes - Dimensions and Weights

Dimensions, wall thickness and weights of stainless steel pipes according to ASME B36.19 Stainless Steel Pipes.

Stainless Steel Weld Fittings - ANSI/ASME B36.19

Dimensions of stainless steel weld fittings according ANSI/ASME B36.19.

Stainless Steels - Corrosion Resistance

Corrosion resistanse of AISI stainless steels in various environments.

Stainless Steels - Identification Tests

Magnetic, spark, hardness and acid identification tests for austenitic, martensitic and ferritic stainless steels.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.