Copper Binary Eutectic Alloys - Melting Points

Sponsored Links

The melting point of an alloy of two (binary) or more metals depends on the relative proportions of the ingredients.

  • an eutectic mixture is the mixture where the melting point is as low as possible

Binary eutectic Copper - Cu - alloys, with composition and melting points are indicated below:

Copper Binary Eutectic Alloys - Melting Points
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Ge - Germanium 37 913 1184
Mg - Magnesium 69.3 758 905
Mn - Manganese 34 1143 1598
Pb - Lead (Plumbum) 36 1230 1755
Pr - Praseodymium 83 745 882
Sb - Antimony (Stibium) 76 800 981
Si - Silicon 16 1075 1476
Te - Tellurium 82 617 207
Ti - Titanium 22 1133 1580
Tl - Thallium 35.3 1357 1983
U - Uranium 25 1213 1724
Zr - Zirconium 13 1253 1796
  • T (oC) = 5/9 (T (oF) - 32)
Sponsored Links

Related Topics

Material Properties

Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Melting and Freezing Points

Melting and freezing points of elements and chemical species at varying conditions.

Related Documents

Copper - Density, Specific Heat and Thermal Conductivity vs. Temperature

Density, specific heat and thermal conductivity of copper vs. temperature

Elements - Melting Points

Melting points of elements.

Fusion and Evaporation Heat of common Materials

Melting points, heat of fusions, boiling points and heat to evaporate common substances - like hydrogen, water, gold and more ..

Gold Binary Eutectic Alloys - Melting Points

Some Au - Gold - binary eutectic alloys and their melting points.

Latent Heat of Melting common Materials

Latent heat of fusion when changing between solid or liquid state for common materials like aluminum, ammonia, glycerin, water and more.

Liquids - Freezing and Melting Points

Common fluids and their freezing and melting points.

Magnesium Binary Eutectic Alloys - Melting Points

Mg - Magnesium - binary eutectic alloys and melting points.

Metal Alloys - Melting Points

Alloys and their melting points.

Metals - Boiling Points and Specific Heat

Boiling points and specific heat of liquid metals.

Metals and Alloys - Melting Temperatures

The melting temperatures for some common metals and alloys.

Molybdenum Binary Eutectic Alloys - Melting Points

Mo - Molybdenum - binary eutectic alloys and melting points.

Salt Hydrates - Melting points and Latent Melting Energy

Melting points and latent energy of salt hydrates.

Solids - Melting and Boiling Temperatures

Melting and boiling temperatures of some products.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.