MetalVapor Pressure (atm)Specific Heat of Liquid
10-310-6
Boiling Point (K)

(cal/goC)(kJ/kgoC)

Aluminum 1782 1333 0.28 1.18
Antimony 1007 741 0.062 0.26
Beryllium 1793 1347 0.78 3.27
Bismuth 1155 851 0.036 0.15
Cadmium 655 486 0.063 0.26
Chromium 1992 1530 0.224 0.94
Cobalt 2167 1652 0.164 0.69
Copper 1862 1391 0.118 0.49
Gold 2023 1510 0.0355 0.15
Iridium 3253 2515 0.043 0.18
Iron 2093 1594 0.197 0.82
Lead 1230 889 0.033 0.14
Magnesium 857 638 0.32 1.34
Manganese 1495 1131 0.20 0.84
Mercury 393 287 0.00
Molybdenum 3344 2558 0.089 0.37
Nickel 2156 1646 0.175 0.73
Niobium (Columbium) 3523 2721 0.083 0.35
Osmium 0.039 0.16
Platinum 2817 2155 0.043 0.18
Plutonium 2200 1596 0.041 0.17
Potassium 606 430
Rhodium 0.092 0.39
Silicon 2340 1749 0.217 0.91
Silver 1582 1179 0.068 0.28
Sodium 701 504 0.00
Tantalum 3959 3052 0.040 0.17
Thorium 3251 2407 0.047 0.20
Tin 1857 1366 0.058 0.24
Titanium 2405 1827 0.188 0.79
Tungsten 4139 3228 0.040 0.17
Uranium 2861 2128 0.048 0.20
Vanadium 2525 1948 0.207 0.87
Zinc 752 559
  • 1 atm = 101325 Pa (N/m2) = 1.013 bar = 14.696 psi (lb/in2) = 760 torr
Sponsored Links

Related Topics

Material Properties

Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Beryllium - Specific Heat vs. Temperatures

Specific heat of beryllium related to temperature.

Copper Binary Eutectic Alloys - Melting Points

Cu - Copper - binary eutectic alloys and their melting points.

Fusion and Evaporation Heat of common Materials

Melting points, heat of fusions, boiling points and heat to evaporate common substances - like hydrogen, water, gold and more ..

Iron Binary Eutectic Alloys - Melting Points

Fe - Iron - binary eutectic alloys and melting points.

Latent Heat of Melting common Materials

Latent heat of fusion when changing between solid or liquid state for common materials like aluminum, ammonia, glycerin, water and more.

Lead Binary Eutectic Alloys - Melting Points

Pb - Lead (Plumbum) - binary eutectic alloys and melting points.

Thermal Conductivity of Metals and Alloys: Data Table & Reference Guide

Thermal conductivities of common metals, metallic elements and alloys.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.