Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

ASTM D3035 - Polyethylene PE pipes - dimensions

Dimensions of PE pipes based on controlled outside diameter.

Dimensions of PE pipes according ASTM D3035 Standard Specification for Polyethylene (PE) Plastic Pipe (DR-PR) Based on Controlled Outside Diameter:

For full table - rotate the screen!

ASTM D3035 - Polyethylene PE pipes - dimensions
Nominal Pipe
Size
(in)
Outside Diameter
(in)
Min. Wall Thickness (in)
DR 32.5DR 26DR 21DR 17DR 15DR 13.5DR 11DR 9.3DR 9DR 7
1/2 0.840 0.062 0.062 0.062 0.062 0.062 0.062 00.076 0.90 0.093 0.120
3/4 1.050 0.062 0.062 0.062 0.062 0.068 0.078 0.095 0.113 0.117 0.150
1 1.315 0.062 0.062 0.063 0.077 0.084 0.097 0.120 0.141 0.146 0.188
1 1/4 1.660 0.062 0.064 0.079 0.098 0.107 0.123 0.151 0.178 0.184 0.237
1 1/2 1.900 0.062 0.073 0.090 0.112 0.123 0.141 0.173 0.204 0.211 0.271
2 2.375 0.073 0.091 0.113 0.140 0.153 0.176 0.216 0.255 0.264 0.339
3 3.500 0.108 0.135 0.167 0.206 0.226 0.259 0.318 0.376 0.389 0.500
4 4.500 0.138 0.173 0.214 0.265 0.290 0.333 0.409 0.484 0.500 0.643
6 6.625 0.204 0.255 0.315 0.390 0.427 0.491 0.602 0.712 0.736 0.946
8 8.625 0.265 0.332 0.411 0.507 0.556 0.639 0.784 0.927 0.958 1.232
10 10.750 0.331 0.413 0.512 0.632 0.694 0.796 0.977 1.156 1.194 1.536
12 12.750 0.392 0.490 0.607 .0750 0.823 0.944 1.159 1.371 1.417 1.821
14 14.000 0.431 0.538 0.667 0.824 0.903 1.037 1.273 1.505 1.556 2.000
16 16.000 0.492 0.615 0.762 0.941 1.032 1.185 1.455 1.720 1.778 2.286
18 18.000 0.554 0.692 0.857 1.059 1.161 1.333 1.636 1.935 2.000 2.571
20 20.000 0.615 0.769 0.952 1.176 1.290 1.481 1.818 2.151 2.222 2.857
22 22.000 0.677 0.846 1.048 1.294 1.419 1.630 2.000 2.366 2.444 3.143
24 24.000 0.738 0.923 1.143 1.412 1.548 1.778 2.182 2.581 2.667 3.429