Minerals and other Materials - Specific Gravities

Sponsored Links
Minerals and other Materials - Specific Gravities
MineralFormulaSpecific Gravity
Andesite 2.8
Barite 4.3
Basalt 2.9
Bauxite 2.4
Biotite complex 2.8 - 3.2
Calcite CaCO3 2.71
Cement clinker 3.1
Cement raw material 2.7
Chrome ore 4.1
Clay 2.2
Clay, calcined 2.3
Coal 1.6
Coke 1.5
Copper ore 3.0
Coral 2.7
Diorite 2.8
Dolomite CaMg(CO3) 2 2.85
Emery 3.5
Feldspar 2.6
Ferrochrome 6.7
Ferromanganese 5.9
Ferrosilicon 4.9
Flint 2.7
Fluorspar 3.0
Gabbro 2.8
Galena 5.4
Garnet 3.3
Glass 2.6
Gneiss 2.7
Gold ore 2.9
Granite 2.7
Graphite 1.8
Gravel 2.7
Gypsum CaSO4.2H2O 2.3
Gypsum rock 2.7
Hematite Fe2O3 5.2 - 5.3
Illite complex 2.6 - 2.86
Ilmenite 4.3
Iron ore 4.0
K Feldspar KAlSi3O8 2.54 - 2.57
Kaolinite Al2Si2O5(OH)4 2.61 - 2.66
Kyanite 3.2
Lead ore 3.4
Lead-zinc ore 3.4
Limestone 2.7
Limestone for cement 2.7
Magnesite, dead burned 5.2
Manganese ore 3.7
Mica 2.9
Molybdenum 2.7
Montmorillonite complex 2.74 - 2.78
Muscovite varies 2.76 - 3.0
Na Feldspar NaAlSi2O8 2.62 - 2.76
Nickel ore 3.3
Oil shale 1.8
Phosphate fertilizer 2.7
Phosphate rock 2.7
Potash ore 2.4
Potash salt 2.2
Pumice 2.0
Pyrite ore 3.5
Pyrrhotite ore 4.0
Quartz SiO2 2.65
Quartz 2.6
Quartzite 2.7
Rutile ore 2.8
Sandstone 2.7
Serpentine Mg3Si2O5(OH)4 2.5 - 2.6
Shale 2.6
Silica 2.7
Silica sand 2.7
Silicon carbide 2.7
Silver ore 2.7
Sinter 3.0
Slag 2.9
Slate 2.5
Sodium silicate 2.1
Spodumene ore 2.8
Syenite 2.7
Tile 2.6
Tin ore 3.9
Titanium ore 4.2
Trap rock 2.9
Uranium ore 2.7
Zinc ore 3.7
Sponsored Links

Related Topics

Material Properties

Material properties of gases, fluids and solids - densities, specific heats, viscosities and more.

Related Documents

Concrete Mixtures

Cement, sand and gravel mixtures.

Density vs. Specific Weight and Specific Gravity

An introduction to density, specific weight and specific gravity.

Geological Time

Geological periods and time scale.

Metal Content in Minerals

Content of metals in minerals.

Mineral Hardness - Mohs Scale

The Mohs qualitative ordinal scale characterizes the scratch resistance of various minerals.

Minerals - Densities

Densities of minerals.

Solids - Densities

Densities of selected solids.

Solids - Specific Heats

Common solids - like brick, cement, glass and many more - and their specific heats - in Imperial and SI units.

Storing Thermal Heat in Materials

Energy stored as sensible heat in materials.

Sponsored Links

Search Engineering ToolBox

  • the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.