Typical content of metals in minerals:

Metal Content in Minerals
MetalMineralContent (%)
Aluminum Bauxit 74
Corundum 53
Spinel 38
Topaz 30
Variscite 17
Wavelite 20
Antimony Allemonite 62
Boulangerite 26
Cervanite 79
jamesonite 29
Meneghinite 19
Miargyrite 41
Niccolite 56
Nickel-Skudderuite 76
Plagionite 38
Polybasite 11
Pyroargyrite 22
Semseyite 27
Stephanite 15
Stibnite 71
Tetrahedrite 30
Zinkenite 45
Arsenic Allemonite 38
Arsenpyrite 34
Loellingite 73
Orpiment 61
Prousite 15
Rammelsbergite 72
Realgar 70
Scrodite 32
Skutterudite 76
Sperrylite 43
Tennantite 20
Barite Barite 59
Whiterite 70
Beryllium Beryl 5
Chrysoberyl 7
Phenakite 16
Birsmuth Bismite 90
Bismuthinite 81
Chromium Chromite 46
Cobalt Cobaltite 36
Erythrite 30
Linaeite 58
Siegenite 15
Skutterudite 18
Smaltite 28
Copper Antlerite 54
Azurite 55
Bornite 63
Brochantite 56
Chalcocite 80
Chalcopyrite 35
Clinoclase 50
Chrysocolla 36
Covellite 66
Cuprite 89
Digenite 78
Malachite 57
Polybasite 12
Stannite 30
Stromeyerite 31
Tennantite 48
Tetrahedrite 35
Torbernite 6
Gold Calaverite 44
Krennerite 44
Petzite 29
Sylvanite 34
Iron Hematite 70
Limonite 60
Mangetite 72
Marcasite 46
Pyrite 46
Pyrrhotite 61
Siderite 48
Triphyllite 35
Troilite 64
Violarite 19
Lead Anglesite 68
Boulangerite 55
Cerussite 77
Galena 87
Meneghenite 62
Minium 91
Phosgenite 76
Plagionite 40
Pyromorphite 76
Semseyite 53
Stolzite 46
Wulfenite 56
Zinkenite 32
Magnesium Magnesite 29
Periclase 60
Spinel 17
Manganese Albandite 63
Braunite 64
Hausmanite 72
Manganoite 77
Pyrolusite 63
Rhodochrosite 48
Rhodonite 48
Tephroite 54
Mercury Calomel 85
Cinnabar 86
Metacinnabarite 86
Molybdenum Molybdenite 60
Powerlite 48
Wulfenite 26
Nickel Annabergite 29
Awaruite 72
Chloanthite 28
Millerite 65
Niccolite 44
Pentlandite 34
Rammelsbergite 28
Siegenite 43
Skutterudite 6
Violarite 39
Silver Acanthite 87
Argentite 87
Bromargyrite 57
Cerargyrite 75
Embolite 70
Hessite 46
Miargyrite 37
Pearceite 77
Petzite 32
Polybasite 60
Proustite 65
Pyrargyrite 60
Stephanite 68
Sternbergite 34
Stromeyerite 53
Sylvanite 6
Tantalium (Ferro)Tantalite 70
Polycrase 15
Samarskite 12
Tin Cassiterite 79
Stannite 28
Titanium Anatase 60
Brookite 60
Ileminte 32
Perovskite 35
Polycrase 15
Rutile 60
Sphene 24
Tungsten Ferberite 90
Huebnerite 61
Scheelite 64
Stolzite 40
Wolframite 60
Uranium U3O8 85
Brannerite 34
Carnotite 53
Phoshuranylite 64
Polycrase 6
Samarsite 16
Skidowskite 55
Torbernite 48
Uraninite 88
Uranophane 41
Vanadium Roscoelite 10
Vanadite 11
V2O5 56
Zinc Calamine 54
Franklinite 16
Gahnite 36
Hydrozincite 60
Smithsonite 52
Sphalerite 64
Willemite 59
Wurtzite 61
Zincite 73
Sponsored Links

Related Topics

Miscellaneous

Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.

Related Documents

Beryllium - Specific Heat vs. Temperatures

Specific heat of beryllium related to temperature.

Mineral Hardness - Mohs Scale

The Mohs qualitative ordinal scale characterizes the scratch resistance of various minerals.

Minerals - Densities

Densities of minerals.

Minerals and other Materials - Specific Gravities

Specific gravities for minerals and other materials.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.