Typical maximum loads on building foundations:

  • Concrete frame, masonry clad : 20 - 25 kN/m2  
  • Steel frame, masonry clad : 15 - 20 kN/m2 
  • Precast concrete floor slabs, masonry walls : 15 - 20 kN/m2
  • Timber frame, masonry clad : 10 - 15 kN/m2
  • Steel frame, steel clad : 5 - 10 kN/m2
Sponsored Links

Related Topics

Miscellaneous

Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.

Related Documents

Concrete Footings - Volume

Estimate required concrete footing volume.

Concrete Mixtures

Cement, sand and gravel mixtures.

Concrete Properties

Properties of normal strength Portland cement concrete.

Concrete Slabs - Required Thickness

Required thickness of concrete slabs.

Floor Joist Capacities

Carrying capacities of domestic timber floor joists - Grade C - metric units.

Floors - Live Loads

Floors and minimum uniformly distributed live loads.

Typical Floor Loads

Uniformly and concentrated floor loads

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.