Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Baume's Hydrometer

Liquid density with Degree Baume vs. Specific Gravity.

The density of a liquid can be measured in degree Baumé.

Note that there are two scales:

  • one for liquids with densities heavier than water
  • one for liquids with densities lighter than water

Note that the relationship between specific gravity and degrees Baumé is a function of the temperature. Different versions of the scale may use different reference temperatures. The table and chart below is based on temperature 60oF (16oC).

Baume's Hydrometer
Degree Baumé Specific Gravity - SG
Heavier than WaterLighter than Water
0 1.000
1 1.007
2 1.014
3 1.021
5 1.036
6 1.043
7 1.051
8 1.058
9 1.066
10 1.074 1.000
11 1.082 0.993
12 1.090 0.986
13 1.099 0.979
14 1.107 0.972
15 1.115 0.966
16 1.124 0.959
17 1.133 0.952
18 1.142 0.946
19 1.151 0.940
20 1.160 0.933
21 1.169 0.927
22 1.179 0.921
23 1.189 0.915
24 1.198 0.909
25 1.208 0.903
26 1.219 0.897
27 1.229 0.892
28 1.239 0.886
29 1.250 0.881
30 1.261 0.875
31 1.272 0.870
32 1.283 0.864
33 1.295 0.859
34 1.306 0.854
35 1.318 0.849
36 1.330 0.843
37 1.343 0.838
38 1.355 0.833
39 1.368 0.828
40 1.381 0.824
41 1.394 0.819
42 1.408 0.814
43 1.422 0.809
44 1.436 0.805
45 1.450 0.800
46 1.465 0.796
47 1.480 0.791
48 1.495 0.787
49 1.510 0.782
50 1.526 0.778
51 1.542 0.773
52 1.559 0.769
53 1.576 0.765
54 1.593 0.761
55 1.611 0.757
56 1.629 0.753
57 1.648 0.749
58 1.667 0.745
59 1.686 0.741
60 1.706 0.737
61 1.726 0.733
62 1.747 0.729
63 1.768 0.725
64 1.790 0.721
65 1.813 0.718
66 1.836 0.714
67 1.859 0.710
68 1.883 0.707
69 1.908 0.704
70 1.933 0.700
71 1.959 0.696
72 1.986 0.693
73 2.014 0.689
74 2.042 0.686
75 2.071 0.683
76 2.101 0.679
77 2.132 0.676
78 2.164 0.673
79 2.197 0.669
80 2.230 0.666

Baume Hydrometer Scale vs. Specific Gravity

Download and print Baume Hydrometer Scale vs. Specific Gravity

Alternative Hydrometer Scales

  • API gravity - used by the petroleum industry
  • Brix scale - used in sugar, fruit juice and wine making industry
  • Oechsle scale - used in brewing and to measure density of grape must
  • Plato scale - used in brewing
  • Twaddell scale - used in the bleaching and dyeing industry

Related Topics

  • Fluid Mechanics

    The study of fluids - liquids and gases. Involving velocity, pressure, density and temperature as functions of space and time.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2010). Baume's Hydrometer. [online] Available at: https://www.engineeringtoolbox.com/degrees-baume-hydrometer-specific-gravity-d_1615.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!