Typical dimensions of threaded ductile-iron pipe pressure class 250 according AWWA C115 Flanged Ductile-Iron Pipe With Ductile-Iron or Gray-Iron Threaded Flanges:

AWWA C115 - Ductile-Iron Threaded Pipe - Dimensions Pressure Class 250
Nominal Size
(inches)
Outside Diameter
(inches)
Thickness
(inches)
3 3.96 0.31
4 4.80 0.32
6 6.90 0.34
8 9.05 0.36
10 11.10 0.38
12 13.20 0.40
14 15.30 0.42
16 17.40 0.43
18 19.50 0.44
20 21.60 0.45
24 25.80 0.47
30 32.00 0.41
36 38.30 0.58
42 44.50 0.65
48 50.80 0.72
54 57.56 0.81
60 61.61 0.83
64 65.67 0.87

Dimensions of Flanges (pressure class 250)

AWWA C115 - Ductile-Iron Threaded Pipe - Dimensions Flanges Pressure Class 250
Nominal Size
(inches)
Outside Flange Diameter
(inches)
Bolt Circle
(inches)
Bolt Hole Diameter
(inches)
Qty. of Bolts
3 7.50 6.00 3/4 4
4 9.00 7.50 3/4 8
6 11.00 9.50 7/8 8
8 13.50 11.75 7/8 8
10 16.00 14.25 1 12
12 19.00 17.00 1 12
14 21.00 18.75 1 1/8 12
16 23.50 21.25 1 1/8 16
18 25.00 22.75 1 1/4 16
20 27.50 25.00 1 1/4 20
24 32.00 29.50 1 3/8 20
30 38.75 36.00 1 3/8 28
36 46.00 42.75 1 5/8 32
42 53.00 49.50 1 5/8 36
48 59.50 56.00 1 5/8 44
54 66.25 62.75 2 44
60 73.00 69.25 2 52
64 80.00 76.00 2 52

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). AWWA C115 - Ductile-Iron Threaded Pipe - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/AWWA-C115-threaded-ductile-iron-pipe-d_2141.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.