Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Butt-Welding Fittings - Dimensions

Butt-Welding Fittings - B16.9 - dimensions.

Dimensions of butt-welding fittings:

Long Radius Elbows

Dimensions Butt-Welding Fittings - Long Radius Elbows
Nominal Pipe Size
(inches)
Outside Pipe Diameter
(inches)
Distance Center to End
(inches)
90o Elbows45o Elbows
1 1.315 1 1/2 7/8
1 1/4 1.660 1 7/8 1
1 1/2 1.900 2 1/4 1 1/8
2 2.375 3 1 3/8
2 1/2 2.875 3 3/4 1 3/4
3 3.5 4 1/2 2
3 1/2 4.0 5 1/4 2 1/4
4 4.5 6 2 1/2
5 5.563 7 1/2 3 1/8
6 6.625 9 3 3/4
8 8.625 12 5
10 10.750 15 6 1/4
  • 1 inch = 25.4 mm

180o Returns

Dimensions Butt-Welding Fittings - 180o Returns
Nominal Pipe Size
(inches)
Outside Pipe Diameter
(inches)
Distance
(inches)
Center to CenterBack to Face
1 1.315 3 2 3/16
1 1/4 1.660 3 3/4 2 3/4
1 1/2 1.900 4 1/2 3 1/4
2 2.375 6 4 3/16
2 1/2 2.875 7 1/2 5 3/16
3 3.5 9 6 1/4
3 1/2 4.0 10 1/2 7 1/4
4 4.5 12 8 1/4
5 5.563 15 10 5/16
6 6.625 18 12 5/16
8 8.625 24 16 5/16
10 10.750 30 20 3/8

Straight Tees

Dimensions Butt-Welding Fittings - Straight Tees
Nominal Pipe Size
(inches)
Outside Pipe Diameter
(inches)
Distance Center to End
(inches)
RunOutlet
1 1.315 1 1/2 1 1/2
1 1/4 1.660 1 7/8 1 7/8
1 1/2 1.900 2 1/4 2 1/4
2 2.375 2 1/2 2 1/2
2 1/2 2.875 3 3
3 3.5 3 3/8 3 3/8
3 1/2 4.0 3 3/4 3 3/4
4 4.5 4 1/8 4 1/8
5 5.563 4 7/8 4 7/8
6 6.625 5 5/8 5 5/8
8 8.625 7 7
10 10.750 8 1/2 8 1/2

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). Butt-Welding Fittings - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/butt-weld-fittings-dimensions-d_1127.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































4.19.9

.