Properties of American Wide Flange Beams according ASTM A6 in metric units are indicated below.

For full table with Static Parameters - Moment of Inertia and Elastic Section Modulus - rotate the screen!

American Wide Flange Beams - Static Parameters
DesignationDimensionsStatic Parameters
Moment of InertiaElastic Section Modulus
Imperal
(in x in x lb/ft)
Metric
(mm x mm x kg/m)
Depth
- h -
(mm)
Width
- w -
(mm)
Web Thickness
- s -
(mm)
Flange Thickness
- f -
(mm)
Sectional Area
(cm2)
Weight
(kg/m)
Ix
(cm4)
Iy
(cm4)
Sx
(cm3)
Sy
(cm3)
W 4 x 4 x 13 W 100 x 100 x 19.3 106 103 7.1 8.8 24.7 19.3 475.9 160.6 89.9 31.2
                     
W 5 x 5 x 16 W 130 x 130 x 23.8 127 127 6.1 9.1 30.4 23.8 885.5 311 139.5 49
W 5 x 5 x 19 W 130 x 130 x 28.1 131 128 6.9 10.9 35.9 28.1 1099 381.4 167.7 59.6
                     
W 6 x 4 x  9 W 150 x 100 x 13.5 150 100 4.3 5.5 17.3 13.5 685.5 91.8 91.4 18.4
W 6 x 4 x 12 W 150 x 100 x 18.0 153 102 5.8 7.1 22.9 18 915.9 125.9 122.1 25.4
W 6 x 4 x 16 W 150 x 100 x 24.0 160 102 6.6 10.3 30.6 24 1342 182.6 167.8 35.8
                     
W 6 x 6 x 15 W 150 x 150 x 22.5 152 152 5.8 6.6 28.6 22.5 1206 386.6 158.6 50.9
W 6 x 6 x 20 W 150 x 150 x 29.8 157 153 6.6 9.3 37.9 29.8 1714 555.5 218.4 72.6
W 6 x 6 x 25 W 150 x 150 x 37.1 162 154 8.1 11.6 47.4 37.1 2220 706.8 274.1 91.8
                     
W 8 x 4 x 10  W 200 x 100 x 15.0 200 100 4.3 5.2 19.1 15 1280 86.9 128 17.4
W 8 x 4 x 13 W 200 x 100 x 19.3 203 102 5.8 6.5 24.8 19.3 1662 115.4 163.7 22.6
W 8 x 4 x 15 W 200 x 100 x 22.5 206 102 6.2 8.0 28.6 22.5 2004 142 194.5 27.8
                     
W 8 x 5.25 x 18 W 200 x 135 x 26.6 207 133 5.8 8.4 33.9 26.6 2587 329.8 250 49.6
W 8 x 5.25 x 21 W 200 x 135 x 31.3 210 134 6.4 10.2 39.7 31.3 3139 409.6 290 61.1
                     
W 8 x 6.5 x 24 W 200 x 165 x 35.9 201 165 6.2 10.2 45.7 35.9 3438 764.3 342.1 92.6
W 8 x 6.5 x 28 W 200 x 165 x 41.7 205 166 7.2 11.8 53.2 41.7 4088 900.5 399 108.5
                     
W 8 x 8 x 31 W 200 x 200 x 46.1 203 203 7.2 11.0 58.9 46.1 4545 1535 448 151.2
W 8 x 8 x 35 W 200 x 200 x 52 206 204 7.9 12.6 66.5 52 5268 1784 512 174.9
W 8 x 8 x 40 W 200 x 200 x 59 210 205 9.1 14.2 75.5 59 6113 2040 582 199.1
W 8 x 8 x 48 W 200 x 200 x 71 216 206 10.2 17.4 91 71 7658 2537 709 246.3
W 8 x 8 x 58 W 200 x 200 x 86 222 209 13 20.6 110 86 9467 3138 853 300.3
W 8 x 8 x 67 W 200 x 200 x 100 229 210 14.5 23.7 127 100 11325 3663 989 348.9
                     
W 10 x 4 x 12 W 250 x 100 x 17.9 251 101 4.8 5.3 22.8 17.9 2254 91.3 179.5 18.1
W 10 x 4 x 15 W 250 x 100 x 22.3 254 102 5.8 6.9 28.5 22.3 2901 122.6 228.4 24
W 10 x 4 x 17 W 250 x 100 x 25.3 257 102 6.1 8.4 32.2 25.3 3430 149.2 266.9 29.3
W 10 x 4 x 19 W 250 x 100 x 28.4 260 102 6.4 10.0 36.3 28.4 3998 177.5 307.5 34.8
                     
W 10 x 5.75 x 22 W 250 x 145 x 32.7 258 146 6.1 9.1 41.9 32.7 4895 472.6 379.4 64.7
W 10 x 5.75 x 26 W 250 x 145 x 38.5 262 147 6.6 11.2 49.1 38.5 6014 593.7 459.1 80.8
W 10 x 5.75 x 30 W 250 x 145 x 44.8 266 148 7.6 13.0 57 44.8 7118 703.5 535.2 95.1
                     
W 10 x 8 x 33 W 250 x 200 x 49.1 247 202 7.4 11.0 62.6 49.1 7069 1513 572.4 149.8
W 10 x 8 x 39 W 250 x 200 x 58 252 203 8.0 13.5 74.2 58 8736 1884 693.4 185.6
W 10 x 8 x 45 W 250 x 200 x 67 257 204 8.9 15.7 85.8 67 10360 2224 806.6 218
                     
W 10 x 10 x 49 W 250 x 250 x 73 253 254 8.6 14.2 92.9 73 11290 3880 892.1 305.5
W 10 x 10 x 54 W 250 x 250 x 80 256 255 9.4 15.6 102 80 12570 4314 982.4 338.3
W 10 x 10 x 60 W 250 x 250 x 89 260 256 10.7 17.3 114 89 14260 4841 1097 378.2
W 10 x 10 x 68 W 250 x 250 x 101 264 257 11.9 19.6 129 101 16380 5549 1241 431.9
W 10 x 10 x 77 W 250 x 250 x 115 269 259 13.5 22.1 146 115 18940 6405 1408 494.6
W 10 x 10 x 88 W 250 x 250 x 131 275 261 15.4 25.1 167 131 22150 7446 1611 570.6
W 10 x 10 x 100 W 250 x 250 x 149 282 263 17.3 28.4 190 149 25940 8622 1840 655.7
W 10 x 10 x 112 W 250 x 250 x 167 289 265 19.2 31.8 212 167 30020 9879 2078 745.6
                     
W 12 x 4 x 14 W 310 x 100 x 21 303 101 5.1 5.7 26.8 21 3708 98.3 244.8 19.5
W 12 x 4 x 16 W 310 x 100 x 23.8 305 101 5.6 6.7 30.4 23.8 4280 115.6 280.7 22.9
W 12 x 4 x 19 W 310 x 100 x 28.3 309 102 6.0 8.9 35.9 28.3 5431 158.1 351.5 31
W 12 x 4 x 22 W 310 x 100 x 32.7 313 102 6.6 10.8 41.8 32.7 6507 191.9 415.8 37.6
                     
W 12 x 6.5 x 26 W 310 x 165 x 38.7 310 165 5.8 9.7 49.4 38.7 8527 726.8 550.1 88.1
W 12 x 6.5 x 30 W 310 x 165 x 44.5 313 166 6.6 11.2 56.7 44.5 9934 854.7 634.8 103
W 12 x 6.5 x 35 W 310 x 165 x 52 317 167 7.6 13.2 66.5 52 11851 1026 747.7 122.9
                     
W 12 x 8 x 40 W 310 x 200 x 60 303 203 7.5 13.1 76.1 60 12860 1829 849 180.8
W 12 x 8 x 45 W 310 x 200 x 67 306 204 8.5 14.6 85.2 67 14510 2069 984 202.8
W 12 x 8 x 50 W 310 x 200 x 74 310 205 9.4 16.3 94.8 74 16450 2344 1061 228.7
                     
W 12 x 10 x 53 W 310 x 250 x 79 306 254 8.8 14.6 101 79 17670 3990 1155 314.2
W 12 x 10 x 58 W 310 x 250 x 86 310 254 9.1 16.3 110 86 19850 4455 1280 350.8
                     
W 12 x 12 x 65 W 310 x 310 x 97 308 305 9.9 15.4 123 97 22240 7286 1444 477.8
W 12 x 12 x 72 W 310 x 310 x 107 311 306 10.9 17.0 136 107 24790 8123 1594 530.9
W 12 x 12 x 79 W 310 x 310 x 117 314 307 11.9 18.7 150 117 27510 9024 1753 587.9
W 12 x 12 x 87 W 310 x 310 x 129 318 308 13.1 20.6 165 129 30770 10040 1935 651.9
W 12 x 12 x 96 W 310 x 310 x 143 323 309 14.0 22.9 182 143 34760 11270 2153 729.4
W 12 x 12 x 106 W 310 x 310 x 158 327 310 15.5 25.1 201 158 38630 12470 2363 804.8
W 12 x 12 x 120 W 310 x 310 x 179 333 313 18.0 28.1 228 179 44530 14380 2675 918.7
W 12 x 12 x 136 W 310 x 310 x 202 341 315 20.1 31.8 257 202 51982 16588 3049 1053
W 12 x 12 x 152 W 310 x 310 x 226 348 317 22.1 35.6 288 226 59560 18930 3423 1194
W 12 x 12 x 170 W 310 x 310 x 253 356 319 24.4 39.6 323 253 68230 21460 3833 1346
W 12 x 12 x 190 W 310 x 310 x 283 365 322 26.9 44.1 360 283 78680 24590 4311 1527
W 12 x 12 x 210 W 310 x 310 x 313 374 325 30.0 48.3 399 313 89560 27700 4789 1705
W 12 x 12 x 230 W 310 x 310 x 342 382 328 32.6 52.6 437 342 100510 31020 5262 1892
  • 1 cm4 = 104 mm4 = 10-8 m4 = 0.024 in4
  • 1 cm3 = 103 mm3 = 10-6 m3 = 0.061 in3
  • 1 cm2 = 102 mm2 = 10-4 m2 =  0.16 in2
  • 1 kg/m = 0.67 lb/ft

Example - Converting Moment of Inertia from cm4 to mm4

The Ix Moment of Inertia of beam W 12 x 12 x 230 is 100510 cm4. It can be converted to mm4 by multiplying with 104 as

(100510 cm4) (104 mm4/cm4) = 1005100000 mm4

                  = 1005 106 mm4

The standard method for specifying the dimensions of a American Wide Flange Beam is for example W 310 x 250 x 79, which is  310 mm deep, 250 mm wide and with a weight of 79 kg/m.

I-shaped cross-section beams:

  • Britain : Universal Beams (UB) and Universal Columns (UC)
  • Europe : IPE. HE. HL. HD and other sections
  • US : Wide Flange (WF) and H sections

Insert beams to your Sketchup model with the Engineering ToolBox Sketchup Extension

w-flange beams sketchup engineering toolbox extension

Related Topics

  • Beams and Columns

    Deflection and stress in beams and columns, moment of inertia, section modulus and technical information.
  • Mechanics

    The relationships between forces, acceleration, displacement, vectors, motion, momentum, energy of objects and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). American Wide Flange Beams. [online] Available at: https://www.engineeringtoolbox.com/american-wide-flange-steel-beams-d_1318.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.3.10

.