Steel Angles - Equal Legs - Dimensions and Static Parameters
Size
(mm x mm)
DimensionsStatic Parameters
Depth
h
(mm)
Thickness
s
(mm)
Sectional Area
(cm2)
Weight
(kg/m)
Moment of Inertia
Ix
(cm4)
25 x 25 25 5 2.26 1.77 1.20
25 4 1.85 1.45 1.01
25 3 1.42 1.11 0.80
30 x 30 30 6 3.27 2.57 2.50
30 5 2.78 2.18 2.16
40 x 40 40 5 4.48 3.52 6.31
40 5 3.79 2.97 4.53
40 4 3.08 2.42 4.47
45 x 45 45 6 5.09 4.00 9.16
45 5 4.30 3.38 7.84
45 4 3.49 2.74 6.43
50 x 50 50 8 7.41 5.82 16.3
50 6 5.69 4.47 12.8
50 5 4.8 3.77 11.0
60 x 60 60 10 11.1 8.69 34.9
60 8 9.03 7.09 29.2
60 6 6.91 5.42 22.8
60 5 5.82 4.57 19.4
70 x 70 70 10 13.1 10.3 57.2
70 8 10.6 8.36 47.5
70 6 8.1 6.38 36.9
80 x 80 80 10 15.1 11.8 87.5
80 8 12.3 9.63 72.2
80 6 9.25 7.34 55.8
90 x 90 90 12 20.3 15.9 148
90 10 17.1 13.4 127
90 8 13.9 10.9 104
90 6 10.6 8.3 80.3
100 x 100 100 15 27.9 21.9 204
100 12 22.7 17.8 207
100 10 19.2 15.0 118
100 8 15.5 12.2 145
120 x 120 120 15 33.9 26.6 445
120 12 27.5 21.6 368
120 10 23.2 18.2 313
120 8 18.7 14.7 255
150 x 150 150 18 51.0 40.1 1050
150 15 43.0 33.8 898
150 12 34.8 27.3 737
150 10 29.3 23.0 624
200 x 200 200 24 90.6 71.1 3330
200 20 76.3 59.9 2850
200 18 69.1 54.2 2600
200 16 61.8 48.5 2340
  • 1 cm4 = 104 mm4 = 10-8 m4 = 0.024 in4
  • 1 cm3 = 103 mm3 = 10-6 m3 = 0.061 in3
  • 1 cm2 = 102 mm2 = 10-4 m2 =  0.16 in2
  • 1 kg/m = 0.67 lb/ft

Related Topics

  • Beams and Columns

    Deflection and stress in beams and columns, moment of inertia, section modulus and technical information.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). Steel Angles - Equal Legs. [online] Available at: https://www.engineeringtoolbox.com/steel-angles-d_1324.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































4.26.8

.