Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Steel Angles - Unequal Legs

Dimensions and static parameters of steel angles with unequal legs - metric units.

steel angle

Properties in imperial units of steel angles with unequal legs are indicated below.

For full table with Static Parameters Moment of Inertia and Section Modulus - rotate the screen!

Steel Angles - Unequal Legs - Dimensions and Static Parameters
Size
(mm x mm)
DimensionsStatic Parameters
Moment of InertiaSection Modulus
Depth
- h -
(mm)
With
- w -
(mm)
Thickness
- s -
(mm)
Sectional Area
(cm2)
Weight
(kg/m)
- Ix -
(cm4)
- Iy -
(cm4)
- Sx -
(cm3)
- Sy -
(cm3)
50 x 40 50 40 6 5.1 3.9 12.1 6.5 3.54 2.35
50 40 5 4.3 3.3 10.3 5.6 3.00 1.99
60 x 30 60 30 6 5.1 4.0 18.2 3.0 4.78 1.32
60 30 5 4.3 3.3 15.6 2.6 4.04 1.12
65 x 50 65 50 8 8.6 8.6 34.8 17.7 7.93 4.9
65 50 6 6.6 6.6 27.2 14.0 6.10 3.8
65 50 5 5.5 5.5 23.2 11.9 5.14 3.2
75 x 50 75 50 10 11.6 11.6 64 22.2 12.8 6.1
75 50 8 9.4 9.4 52 18.4 10.4 4.9
75 50 6 7.2 7.2 41 14.4 8.0 3.8
80 x 60 80 60 8 10.6 10.6 66 31.8 12.2 7.2
80 60 7 9.4 9.4 59 28.4 10.7 6.3
80 60 6 8.1 8.1 51 24.8 9.3 5.5
100 x 65 100 65 10 15.6 15.6 154 51 23.2 10.5
100 65 8 12.7 12.7 127 42 18.9 8.5
100 65 7 11.2 11.2 113 38 16.6 7.5
100 x 75 100 75 12 19.7 19.7 189 90 28.0 16.5
100 75 10 16.6 16.6 162 78 23.8 14.0
100 75 8 13.5 13.5 133 64 19.3 11.4
125 x 75 125 75 12 22.7 22.7 354 96 43.2 16.9
125 75 10 19.1 19.1 302 82 36.5 14.3
125 75 8 15.5 15.5 247 68 29.6 11.6
150 x 75 150 75 15 31.6 31.6 713 120 75 21.0
150 75 12 25.7 25.7 589 100 61 17.2
150 75 10 21.6 21.6 501 86 52 14.6
150 x 90 150 90 15 33.9 33.9 761 205 78 30.4
150 90 12 27.5 27.5 927 171 63 24.8
150 90 10 23.2 23.2 533 146 53 21.0
200 x 100 200 100 15 43 43 1758 299 137 38.4
200 100 12 34.8 34.8 1440 247 111 31.3
200 100 10 29.2 29.2 1220 210 93 26.3
200 x 150 200 150 18 60.0 60 2376 1146 174 103
200 150 15 50.5 50.5 2022 976 147 87
200 150 12 40.8 40.8 1652 803 119 71
  • 1 in = 25.4 mm
  • 1 cm4 = 10-8 m = 104 mm
  • 1 in4 = 4.16x105 mm4 = 41.6 cm4
  • 1 cm3 = 10-6 m3 = 103 mm3

Related Topics

  • Beams and Columns

    Deflection and stress in beams and columns, moment of inertia, section modulus and technical information.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). Steel Angles - Unequal Legs. [online] Available at: https://www.engineeringtoolbox.com/steel-angles-unequal-legs-d_1325.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































4.26.8

.