Dimensions of PVC pipes with structured walls according EN 1453.

Dimensions of PVC pipes according EN 1453Plastics piping systems with structured-wall pipes for soil and waste discharge (low and high temperature) inside buildings. Unplasticized poly (vinyl chloride) (PVC-U). Specifications for pipes and the system:

EN 1453 - PVC Piping with Structured Walls - Dimensions
Nominal Size
(mm)
Nominal Outside Diameter
(mm)
Wall Thickness
(mm)
32 32 3.2
40 40 3.2
50 50 3.2
63 63 3.2
75 75 3.2
100 100 3.2
125 125 3.2
140 140 3.6
160 160 4.0
200 200 4.9

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). EN 1453 - PVC Piping with Structured Walls - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/EN-1453-PVC-pipes-structured-wall-d_2132.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.3.10

.