EN 1329 - PVC Piping for Soil and Waste Discharge - Dimensions

Dimensions of PVC pipes according EN 1329.

Dimensions of EN 1329 Plastics piping systems for soil and waste discharge (low and high temperature) within the building structure. Unplasticized poly(vinyl chloride) (PVC-U):

Metric Series

EN 1329 - PVC Piping for Soil and Waste Discharge - Dimensions Metric Series
Nominal Size
(mm)
Nominal Outside Diameter
(mm)
Mean Outside Diameter (mm)
minmax
32 32 32.0 32.2
40 40 40.0 40.2
50 50 50.0 50.2
63 63 63.0 63.2
75 75 75.0 75.3
80 80 80.0 80.3
82 82 82.0 82.3
90 90 90.0 90.3
100 100 1000.0 100.3
110 110 110.0 110.3
125 125 125.0 125.3
140 140 140.0 140.4
160 160 160.0 160.4
180 180 180.0 180.4
200 200 200.0 200.5
250 250 250.0 250.5
315 315 315.0 315.6

Inch based Series

EN 1329 - PVC Piping for Soil and Waste Discharge - Dimensions Imperial Series
Nominal Size
(mm)
Nominal Outside Diameter
(mm)
Mean Outside Diameter (mm)
minmax
36 36 36.2

36.5

43 43 42.8 43.1
56 56 55.8 56.1

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). EN 1329 - PVC Piping for Soil and Waste Discharge - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/EN-1329-pvc-plastic-pipes-d_2130.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.3.10

.