EN 1452 - Unplasticized Poly Vinyl Chloride (PVC-U) - Dimensions
Nominal Outside Diameter
(mm)
Min. Wall Thickness (mm)
S 20
SDR 41
S 16.7
SDR 34.4
S 16
SDR 33
S 12.5
SDR 26
S 10
SDR 21
S 8
SDR 17
S 6.3
SDR 13.6
S 5
SDR 11
Nominal Pressure PN (design coefficient 2.5)
PN 6 PN 6 PN 8 PN 10 PN 12.5 PN 16 PN 20
12 1.5
16 1.5
20 1.5 1.9
25 1.5 1.9 2.3
32 1.5 1.6 1.9 2.4 2.9
40 1.5 1.6 1.9 2.4 3.0 3.7
50 1.6 2.0 2.4 3.0 3.7 4.6
63 2.0 2.5 3.0 3.8 4.7 5.8
75 2.3 2.9 3.6 4.5 5.6 6.8
90 2.8 3.5 4.3 5.4 6.7 8.2
Nominal Pressure PN (design coefficient 2.0)
PN 6.3 PN 7.5 PN 8 PN 10 PN 12.5 PN 16 PN 20 PN 25
63 2.0 2.0 2.4 3.0 3.8
75 2.0 2.2 2.9 3.6 4.5
90 2.0 2.7 3.5 4.3 5.4
Nominal Pressure PN (design coefficient 2.0)
PN 6 PN 7.5 Pn 8 PN 10 PN 12.5 PN 16 PN 20 PN 25
110 2.7 3.2 3.4 4.2 5.3 6.6 8.1 10.0
125 3.1 3.7 3.9 4.8 6.0 7.4 9.2 11.4
140 3.5 4.1 4.3 5.4 6.7 8.3 10.3 12.7
160 4.0 4.7 4.9 6.2 7.7 9.5 11.8 14.6
180 4.4 5.3 5.5 6.9 8.6 10.7 13.3 16.4
200 4.9 5.9 6.2 7.7 9.6 11.9 14.7 18.2
225 5.5 6.6 6.9 8.6 10.8 13.4 16.6
250 6.2 7.3 7.7 9.6 11.9 14.8 18.4
280 6.9 8.2 8.6 10.7 13.4 16.6 20.6
315 7.7 9.2 9.7 12.1 15.0 18.7 23.2
355 8.7 10.4 10.9 13.6 16.9 21.1 26.1
400 9.8 11.7 12.3 45.3 19.1 23.7 29.4
450 11.0 13.2 13.8 17.2 21.5 26.7 33.1
500 12.3 14.6 15.3 19.1 23.9 29.7 36.8
560 13.7 16.4 17.2 21.4 26.7
630 15.4 18.4 19.3 24.1 30.0
710 17.4 20.7 21.8 27.2
800 19.6 23.3 24.5 30.6
900 22.0 26.3 27.6
1000 24.5 29.2 30.6

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). EN 1452 - Unplasticized Poly Vinyl Chloride (PVC-U) - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/EN-1452-PVC-U-pipes-d_2142.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.3.10

.