Nominal SizesExternal DiameterExternal Diameter ToleranceMinimum Wall ThicknessWall Thickness Tolerance
DNmminchmmmmmmmm
10 12 3/8 12 0.08 1.0 0.13
15 15 0.08 1.0 0.13
15 18 1/2 18 0.08 1.0 0.13
20 22 3/4 22 0.12 1.0 0.13
25 28 1 28 0.12 1.5 0.13
32 35 1 1/4 35 0.15 1.5 0.13
40 42 1 1/2 42 0.15 1.5 0.13
50 54 2 54 0.20 2.0 0.13
65 76.1 2 1/2 76.1 0.20 2.0 0.13
80 88.9 3 88.9 0.20 2.0 0.13
100 108 4 108 0.50 2.5 0.13

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2017). EN 12449 - Copper and Copper Alloys - Seamless, Round Tubes for General Purposes - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/en-12449-copper-tubes-dimensions-d_11.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.8.12

.