CPVC Tubes - Pressure and Temperature Ratings

CTS (Copper Tube Sized) CPVC (Chlorinated Poly Vinyl Chloride) tubes temperature and pressure ratings.

Pressure and temperature de-rating factors for CTS (Copper Tube Size) and CPVC1) (Chlorinated Poly Vinyl Chloride) tubes according ASTM D2846 - CPVC Plastic Hot and Cold Water Distribution Tubes - Dimensions :

CPVC Tubes - Pressure and Temperature De-rating
Temperature
(oF)
De-Rating FactorRating
(psi)
73 1.00 400
80 1.00 400
90 0.91 360
100 0.82 325
120 0.65 260
140 0.50 200
160 0.40 160
180 0.25 100

1)Chlorinated Poly Vinyl Chloride (CPVC) is a thermoplastic pipe and fitting material made with CPVC compounds meeting the requirements of ASTM Class 23447 as defined in ASTM Specification D1784. CPVC applications are for potable water distribution, corrosive fluid handling in industry, and fire suppression systems.

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2010). CPVC Tubes - Pressure and Temperature Ratings. [online] Available at: https://www.engineeringtoolbox.com/cts-cpvc-tubes-pressure-ratings-d_1665.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.3.10

.