Nominal Pipe Size
(in)
Average Outside Diameter
(in)
Minimum Wall Thickness (in)
SDR 64SDR 41SDR 32.5SDR 26SDR 21SDR 17SDR 13.5
1/8 0.405 0.060
1/4 0.540 0.060
3/8 0.675 0.060
1/2 0.840 0.062
3/4 1.050 0.060 0.062 0.078
1 1.315 0.060 0.063 0.077 0.097
1 1/4 1.660 0.060 0.064 0.079 0.098 0.123
1 1/2 1.900 0.060 0.073 0.090 0.112 0.141
2 2.375 0.073 0.091 0.113 0.140 0.176
2 1/2 2.875 0.088 0.110 0.137 0.169 0.213
3 3.500 0.085 0.108 0.135 0.167 0.206 0.259
3 1/2 4.000 0.098 0.123 0.154 0.190 0.235 0.296
4 4.500 0.070 0.110 0.138 0.173 0.214 0.265 0.333
5 5.563 0.087 0.136 0.171 0.214 0.265 0.327 0.412
6 6.625 0.104 0.162 0.204 0.255 0.316 0.390 0.491
8 8.625 0.135 0.210 0.265 0.332 0.410 0.508
10 10.750 0.168 0.262 0.331 0.413 0.511 0.632
12 12.750 0.199 0.311 0.392 0.490 0.606 0.750
14 14.000 0.341 0.430 0.538 0.666 0.823
16 16.000 0.390 0.492 0.615 0.762 0.941
18 18.000 0.439 0.554 0.692 0.857 1.059
20 20.000 0.488 0.615 0.769 0.952 1.176
24 24.000 0.585 0.738 0.923 1.143 1.412
30 30.000 0.732 0.923 1.154 1.428 1.765
36 36.000 0.878 1.108 1.385 1.714 2.118

For sizes 1 1/4" and larger ASTM D2665 for DWV pipe is comparable to ASTM D1785 Schedule 40.

PVC pipes - SDR series vs. wall thickness and dimension

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). ASTM D2241 - Poly(Vinyl Chloride) (PVC) Pressure-Rated Pipe (SDR Series) - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/ASTM-D2241-pvc-sdr-pipe-d_2129.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.3.10

.