Ethane Liquid - C2H6 - Thermal Properties
Temperature
- T -
(K)
Pressure
- p -
(kPa)
Enthalpy
- h -
(kJ/kg)
Entropy
- s -
(kJ/(kg K))
Specific Heat Capacity
- cv -
(kJ/(kg K))
Specific Heat
- cp -
(kJ/(kg K))
Speed of Sound
- c -
(m/s)
Density
- ρ -
(kg/m3)
90.368
(triple point)
0.0011 -889 -5.06 1.61 2.33 2008 652
120 0.352 -821 -4.41 1.48 2.28 1794 619
150 9.64 -752 -3.90 1.44 2.33 1576 585
160 21.4 -729 -3.75 1.44 2.36 1501 574
170 42.8 -705 -3.60 1.43 2.39 1426 562
180 78.6 -681 -3.46 1.43 2.42 1350 550
184 98.3 -671 -3.41 1.44 2.44 1320 545
Standard Temperature and Pressure
186 109.4 -666 -3.38 1.44 2.45 1305 542
190 134.6 -656 -3.33 1.44 2.46 1274 537
200 217.2 -631 -3.21 1.44 2.51 1196 524
210 333.8 -606 -3.08 1.45 2.57 1117 510
220 492.1 -580 -2.96 1.47 2.65 1037 496
230 700.2 -553 -2.84 1.49 2.73 956 481
240 966.8 -525 -2.73 1.51 2.85 873 465
250 1301 -496 -2.61 1.53 2.99 788 448
260 1711 -465 -2.49 1.57 3.20 701 429
270 2210 -432 -2.38 1.61 3.49 609 408
280 2807 -397 -2.25 1.65 3.99 512 383
300 4357 -305 -1.95 1.91 10.02 275 304
305.322
(critical point)
4872 -230.7 -1.71 206

Ethane is an organic chemical compound with chemical formula C2H6.

Related Topics

  • Material Properties

    Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2011). Ethane Liquid - Thermal Properties. [online] Available at: https://www.engineeringtoolbox.com/ethane-thermal-properties-d_1761.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































4.26.8

.