Nickel and Nickel Alloy Pipes - Temperature Ranges

Temperature ranges for bending nickel and nickel alloy pipes and tubes.

Temperature ranges for hot bending nickel and nickel alloy pipes and tubes:

Nickel and Nickel Alloy Pipes - Temperature Ranges
Copper or Copper AlloyTemperature Range
(oF)

Nickel 1200 - 2300
Nickel Copper 1700 - 2150
Ni-Cr-Fe 1850 - 2300
Ni-Fe-Cr 1850 - 2200
Low Carbon Nickel 1200 - 2300
  • T(oC) = 5/9[T(oF) - 32]

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2005). Nickel and Nickel Alloy Pipes - Temperature Ranges. [online] Available at: https://www.engineeringtoolbox.com/hot-bending-nickel-pipe-d_862.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.8.12

.