MineralFormulaSpecific Gravity
Andesite 2.8
Barite 4.3
Basalt 2.9
Bauxite 2.4
Biotite complex 2.8 - 3.2
Calcite CaCO3 2.71
Cement clinker 3.1
Cement raw material 2.7
Chrome ore 4.1
Clay 2.2
Clay, calcined 2.3
Coal 1.6
Coke 1.5
Copper ore 3.0
Coral 2.7
Diorite 2.8
Dolomite CaMg(CO3) 2 2.85
Emery 3.5
Feldspar 2.6
Ferrochrome 6.7
Ferromanganese 5.9
Ferrosilicon 4.9
Flint 2.7
Fluorspar 3.0
Gabbro 2.8
Galena 5.4
Garnet 3.3
Glass 2.6
Gneiss 2.7
Gold ore 2.9
Granite 2.7
Graphite 1.8
Gravel 2.7
Gypsum CaSO4.2H2O 2.3
Gypsum rock 2.7
Hematite Fe2O3 5.2 - 5.3
Illite complex 2.6 - 2.86
Ilmenite 4.3
Iron ore 4.0
K Feldspar KAlSi3O8 2.54 - 2.57
Kaolinite Al2Si2O5(OH)4 2.61 - 2.66
Kyanite 3.2
Lead ore 3.4
Lead-zinc ore 3.4
Limestone 2.7
Limestone for cement 2.7
Magnesite, dead burned 5.2
Manganese ore 3.7
Mica 2.9
Molybdenum 2.7
Montmorillonite complex 2.74 - 2.78
Muscovite varies 2.76 - 3.0
Na Feldspar NaAlSi2O8 2.62 - 2.76
Nickel ore 3.3
Oil shale 1.8
Phosphate fertilizer 2.7
Phosphate rock 2.7
Potash ore 2.4
Potash salt 2.2
Pumice 2.0
Pyrite ore 3.5
Pyrrhotite ore 4.0
Quartz SiO2 2.65
Quartz 2.6
Quartzite 2.7
Rutile ore 2.8
Sandstone 2.7
Serpentine Mg3Si2O5(OH)4 2.5 - 2.6
Shale 2.6
Silica 2.7
Silica sand 2.7
Silicon carbide 2.7
Silver ore 2.7
Sinter 3.0
Slag 2.9
Slate 2.5
Sodium silicate 2.1
Spodumene ore 2.8
Syenite 2.7
Tile 2.6
Tin ore 3.9
Titanium ore 4.2
Trap rock 2.9
Uranium ore 2.7
Zinc ore 3.7

Related Topics

  • Material Properties

    Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2010). Minerals and other Materials - Specific Gravities. [online] Available at: https://www.engineeringtoolbox.com/minerals-specific-gravity-d_1644.html [Accessed Day Month Year].