EN 13348 Seamless, Round Copper Tubes for Medical Gases or Vacuum - Dimensions

Dimensions of seamless round copper and copper alloys tubes for medical gases or vacuum.

Dimensions of copper tubes according EN 13348 Copper and copper alloys. Seamless, round copper tubes for medical gases or vacuum:

EN 13348 Seamless, Round Copper Tubes for Medical Gases or Vacuum - Dimensions
Nominal Outside Diameter
- d -
(mm)
Nominal Wall Thickness - e - (mm)
0.50.60.70.80.91.01.11.21.52.02.53.0
12
15
22
28
35
42
54
66.7
76.1
108
133
159
219

Recommended

  • 1 inch = 25.4 mm

Example - Designation of EN 13348 Copper Tube

  • Copper tube EN 13348 R290 15×1.0

where R290 is material temper.

Material Temper

Copper tube EN 13348 - Hardness and Strength
Material TemperTensile StrengthElongation min.Vickers Hardness
DesignationCommonly used term(MPa)(%)HV5
R250 half hard 250 30, 20 75 - 100
R290 hard 290 3 over 100

EN 1173 - Letter symbols for Property Designations

  • A Elongation
  • B Spring bending limit
  • G Grain size
  • H Hardness (Brinell for castings, Vickers for wrought products)
  • M (as) Manufactured, i.e. without specified mechanical properties
  • R Tensile strength (like R250 - 250 MPa)
  • Y 0.2% proof strength

Typical Available Dimensions

Plain Straight Tubes

Copper tube EN 13348 - Typical Available Dimensions
Nominal Outside Diameter
(mm)
Tube Length
(m)
Wall Thickness
(mm)
12 6 0.6
15 3, 6 0.7
22 3, 6 0.9
28 3, 6 0.9
35 6 1.0
42 6 1.0
54 6 1.0
67 6 1.5
76 6 1.5
108 6 1.5
133 6 1.5
159 6 2.0
219 6 3.0

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). EN 13348 Seamless, Round Copper Tubes for Medical Gases or Vacuum - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/EN-13348-seamless-round-copper-tubes-for-medical-gases-or-vacuum-d_2126.html [Accessed Day Month Year].