EN 12735 Seamless, Round Copper Tubes for Air Conditioning and Refrigeration - Dimensions

Dimensions of seamless, round copper tubes for air conditioning and refrigeration piping systems.

Dimensions of copper tubes according EN 12735 Copper and copper alloys. Seamless, round copper tubes for air conditioning and refrigeration. Tubes for piping systems:

EN 12735 Seamless, Round Copper Tubes for Air Conditioning and Refrigeration - Dimensions
Nominal Outside Diameter
- d -
Nominal Wall Thickness - e - (mm)
Metric SeriesImperial Series
(mm)(mm)(in)0.81.01.251.51.652.02.5
3.18 1/8 C
3.97 5/32 C C
4.76 3/16 C
6 S, C C
6.35 1/4 C C
7.94 5/16 C C
8 S, C C
9.52 3/8 C C
10 S, C S, C
12 S, C
12.7 1/2 C S, C
15 S, C
15.87 5/8 S, C
18 S, C
19.06 3/4 C S
22 S, C
22.3 7/8 C S
25.4 1 S
28 S
28.57 1 1/8 S S
34.92 1 3/8 S
35 S
41.27 1 5/8 S
42 S
53.97 2 1/8 S S
54 S
64 S
66.67 2 5/8 S S S
76.1 S
79.37 3 1/8 S S
88.90 3 1/2 S
92.07 3 5/8 S S
104.80 4 1/8 S S
108 S

Recommended

  • S - available in straight lengths
  • C - available in coils
  • 1 inch = 25.4 mm

Example - Designation of EN 12735 Copper Tube

  • Copper tube EN 12735 R290 15×1.0

where R290 is material temper.

Material Temper

EN 12735 Seamless, Round Copper Tubes for Air Conditioning and Refrigeration - Material Temper
Material TemperTensile StrengthElongation min.Vickers Hardness
DesignationCommonly used term(MPa)(%)HV5
R220 annealed, soft 40 40 - 70
R250 half hard 250 30 75 - 100
R290 hard 290 3 over 100

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). EN 12735 Seamless, Round Copper Tubes for Air Conditioning and Refrigeration - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/EN-12735-copper-tubes-air-conditioning-refrigeration-d_2127.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.