Wire Gauge

SWG - Standard Wire Gauge - Diameter
Standard Wire Gauge
SWG
Diameter
inchesmm
7/0 0.500 12.700
6/0 0.464 11.786
5/0 0.432 10.973
4/0 0.400 10.160
3/0 0.372 9.449
2/0 0.348 8.839
1/0 0.324 8.236
1 0.300 7.620
2 0.276 7.010
3 0.252 6.401
4 0.232 5.893
5 0.212 5.385
6 0.192 4.877
7 0.176 4.470
8 0.160 4.064
9 0.144 3.658
10 0.128 3.251
11 0.116 2.946
12 0.104 2.642
13 0.092 2.337
14 0.080 2.032
15 0.072 1.829
16 0.064 1.626
17 0.056 1.422
18 0.048 1.219
19 0.040 1.016
20 0.036 0.914
21 0.032 0.813
22 0.028 0.711
23 0.024 0.610
24 0.022 0.559
25 0.020 0.508
26 0.018 0.457
27 0.0164 0.417
28 0.0148 0.376
29 0.0136 0.345
30 0.0124 0.315
31 0.0116 0.295
32 0.0108 0.274
33 0.0100 0.254
34 0.0092 0.234
35 0.0084 0.213
36 0.0076 0.193
37 0.0068 0.173
38 0.006 0.152
39 0.0052 0.132
40 0.0048 0.122
41 0.0044 0.112
42 0.004 0.102
43 0.0036 0.091
44 0.0032 0.081
45 0.0028 0.071
46 0.0024 0.061
47 0.002 0.051
48 0.0016 0.041
49 0.0012 0.030
50 0.001 0.025

The Standard Wire Gauge (SWG) series commonly used in Great Britain were given in BS 3737: 1964. The standard is now withdrawn. The basis of the system is the mil, or 0.001 inches.

Related Topics

  • Electrical

    Electrical engineering with units, amps and electrical wiring. Wire gauges, electrical formulas, motors and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2011). SWG - Standard Wire Gauge. [online] Available at: https://www.engineeringtoolbox.com/swg-standard-wire-gauge-d_1779.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.