Pipes - Nominal Wall Thickness

Nominal wall thickness of seamless and welded carbon and alloy steel pipes

Nominal wall thickness for seamless and welded steel pipes according ANSI B36.10:

For full table with higher Schedules - rotate the screen!

Pipes - Nominal Wall Thickness
NPS
(in)
Outside Diameter
(in)
Schedule
102030STD4060XS80100120140160XXS
Wall Thickness (in)
1/8 0.405       0.068 0.068   0.095 0.095          
1/4 0.540       0.088 0.088   0.119 0.119          
3/8 0.675       0.091 0.091   0.126 0.126          
1/2 0.840       0.109 0.109   0.147 0.147       0.187 0.294
3/4 1.050       0.113 0.113   0.154 0.154       0.219 0.308
1 1.315       0.133 0.133   0.179 0.179       0.250 0.358
1 1/4 1.660       0.140 0.140   0.191 0.191       0.250 0.382
1 1/2 1.900       0.145 0.145   0.200 0.200       0.281 0.400
2 2.375       0.154 0.154   0.218 0.218       0.344 0.436
2 1/2 2.875       0.203 0.203   0.276 0.276       0.375 0.552
3 3.500       0.216 0.216   0.300 0.300       0.438 0.600
3 1/2 4.000       0.226 0.226   0.318 0.318          
4 4.500       0.237 0.237   0.337 0.337   0.438   0.531 0.674
5 5.563       0.258 0.258   0.375 0.375   0.500   0.625 0.750
6 6.625       0.280 0.280   0.432 0.432   0.562   0.719 0.864
8 8.625   0.250 0.277 0.322 0.322 0.406 0.500 0.500 0.594 0.719 0.812 0.906 0.875
10 10.750   0.250 0.307 0.365 0.365 0.500 0.500 0.594 0.719 0.844 1.000 1.125 1.000
12 12.750   0.250 0.330 0.375 0.406 0.562 0.500 0.688 0.844 1.000 1.125 1.312 1.000
14 14.000 0.250 0.312 0.375 0.375 0.438 0.594 0.500 0.750 0.938 1.094 1.250 1.406  
16 16.000 0.250 0.312 0.375 0.375 0.500 0.656 0.500 0.844 1.031 1.219 1.438 1.594  
18 18.000 0.250 0.312 0.438 0.375 0.562 0.750 0.500 0.938 1.156 1.375 1.562 1.781  
20 20.000 0.250 0.375 0.500 0.375 0.594 0.812 0.500 1.031 1.281 1.500 1.750 1.969
22 22.000 0.250 0.375 0.500 0.375 0.875 0.500 1.125 1.375 1.625 1.875 2.125
24 24.000 0.250 0.375 0.562 0.375 0.688 0.969 0.500 1.219 1.531 1.812 2.062 2.344
30 30.000 0.312 0.500 0.625 0.375 0.500
32 32.000 0.312 0.500 0.625 0.375 0.688
34 34.000 0.312 0.500 0.625 0.375 0.688
36 36.000 0.312 0.500 0.625 0.375 0.750
42 42.000 0.500 0.625 0.375 0.750
  • STD - Standard
  • XS - Extra Strong
  • XXS - Double Extra Strong

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). Pipes - Nominal Wall Thickness. [online] Available at: https://www.engineeringtoolbox.com/nominal-wall-thickness-pipe-d_1337.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.