HEMDimensionsStatic Parameters
Moment of InertiaElastic Section Modulus
Depth
h
(mm)
Width
w
(mm)
Web Thickness
s
(mm)
Sectional Area
(cm2)
Weight
(kg/m)
Ix
(cm4)
Iy
(cm4)
Sx
(cm3)
Sy
(cm3)
100M 120 106 12 53.2 41.8 1140 399 190 75.3
120M 140 126 12.5 66.4 52.1 2020 703 288 112
140M 160 146 13 80.6 63.2 3290 1140 411 157
160M 180 166 14 97.1 76.2 5100 1760 566 212
180M 200 186 14.5 113 88.9 7480 2580 748 277
200M 220 206 15 131 103 10640 3650 967 354
220M 240 226 15.5 149 117 14600 5010 1220 444
240M 270 248 18 200 157 24290 8150 1800 657
260M 290 268 18 220 172 31310 10450 2160 780
280M 310 288 18.5 240 189 39550 13160 2550 914
300M 340 310 21 303 238 59200 19400 3480 1250
320M 359 309 21 312 245 68130 19710 3800 1280
340M 377 309 21 316 248 76370 19710 4050 1280
  • 1 cm4 = 104 mm4 = 10-8 m4 = 0.024 in4
  • 1 cm3 = 103 mm3 = 10-6 m3 = 0.061 in3
  • 1 cm2 = 102 mm2 = 10-4 m2 =  0.16 in2
  • 1 kg/m = 0.67 lb/ft

I-shaped cross-section beams:

  • Britain : Universal Beams (UB) and Universal Columns (UC)
  • Europe : IPE. HE. HL. HD and other sections
  • US : Wide Flange (WF) and H sections

Related Topics

  • Beams and Columns

    Deflection and stress in beams and columns, moment of inertia, section modulus and technical information.
  • Mechanics

    The relationships between forces, acceleration, displacement, vectors, motion, momentum, energy of objects and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). HE-M Steel Beams. [online] Available at: https://www.engineeringtoolbox.com/he-m-steel-beams-d_1315.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.