Standard dimensions for seamless red brass pipe according ASTM B4:

Regular

ASTM B43 - Seamless Red Brass Pipes - Dimensions - Regular
Nominal SizeOutside DiameterWall ThicknessWeight
(in)(in)(mm)(in)(mm)(lb/ft)(kg/m)
1/8 0.405 10.3 0.062 1.57 0.253 0.376
1/4 0.540 13.7 0.082 2.08 0.447 0.665
3/8 0.675 17.1 0.090 2.29 0.627 0.993
1/2 0.840 21.3 0.107 2.72 0.934 1.39
3/4 1.050 26.7 0.114 2.90 1.27 1.89
1 1.315 33.4 0.126 3.20 1.78 2.65
1 1/4 1.660 42.2 0.146 3.71 2.63 3.91
1 1/2 1.900 48.3 0.150 3.81 3.13 4.66
2 2.375 60.3 0.156 3.96 4.12 6.13
2 1/2 2.875 73.0 0.187 4.75 5.99 8.91
3 3.500 88.9 0.219 5.56 8.56 12.7
3 1/2 4.000 102 0.250 6.35 11.2 16.7
4 4.500 114 0.250 6.35 12.7 18.9
5 5.562 141 0.250 6.35 15.8 23.5
6 6.625 168 0.250 6.35 19.0 28.3
8 8.625 219 0.312 7.92 30.9 46.0
10 10.750 273 0.365 9.27 45.2 67.3
12 12.750 324 0.375 9.52 55.3 82.3

Extra Strong

ASTM B43 - Seamless Red Brass Pipes - Dimensions - Extra Strong
Nominal SizeOutside DiameterWall ThicknessWeight
(in)(in)(mm)(in)(mm)(lb/ft)(kg/m)
1/8 0.405 10.3 0.100 2.54 0.363 0.540
1/4 0.540 13.7 0.123 3.12 0.611 0.909
3/8 0.675 17.1 0.127 3.23 0.829 1.23
1/2 0.840 21.3 0.149 3.78 1.23 1.83
3/4 1.050 26.7 0.157 3.99 1.67 2.48
1 1.315 33.4 0.182 4.62 2.46 3.66
1 1/4 1.660 42.2 0.194 4.93 3.39 5.04
1 1/2 1.900 48.3 0.203 5.16 4.10 6.10
2 2.375 60.3 0.221 5.61 5.67 8.44
2 1/2 2.875 73.0 0.280 7.11 8.66 12.9
3 3.500 88.9 0.304 7.72 11.6 17.3
3 1/2 4.000 102 0.321 8.15 14.1 21.0
4 4.500 114 0.341 8.66 16.9 25.1
5 5.562 141 0.375 9.52 23.2 34.5
6 6.625 168 0.437 11.1 32.2 47.9
8 8.625 219 0.500 12.7 48.4 72.0
10 10.750 273 0.500 12.7 61.1 90.9

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). ASTM B43 - Seamless Red Brass Pipes - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/b43-red-brass-pipe-seamless-d_2121.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.