Nominal DiameterActual Outside DiameterInside DiameterWall ThicknessWeight
(inches)(mm)(inches)(mm)(inches)(mm)(inches)(mm)(lbs/ft)(kg/m)
1/2 15 0.840 21.3 0.710 18.0 0.065 1.7 0.6 0.9
3/4 20 1.050 26.9 0.920 23.4 0.065 1.7 0.7 1.1
1 25 1.315 33.7 1.185 30.1 0.065 1.7 0.9 1.3
1 1/4 32 1.660 42.4 1.530 38.9 0.065 1.7 1.1 1.6
1 1/2 40 1.900 48.3 1.770 45.0 0.065 1.7 1.3 1.9
2 50 2.375 60.3 2.2245 57.0 0.065 1.7 1.6 2.4

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). Pressfit Piping - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/pressfit-piping-dimensions-d_1166.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.