Number of Wire GaugeU.S. Standard Gauge for Sheet and Plate Iron and Steel
(in)
Stubs' Iron Wire
(in)
American or Brown & Sharpe
(in)
Birmingham Iron Wire
(in)
Washburn & Moen or Steel Wire Gauge
(in)
Music Wire Gauge
(in)
Stubs' Steel Wire
(in)
0000000 0.50       0.490    
000000 0.469   0.580   0.462 0.004  
00000 0.436   0.517   0.431 0.005  
0000 0.406 0.454 0.460 0.454 0.394 0.006  
000 0.375 0.425 0.410 0.425 0.363 0.007  
00 0.344 0.380 0.365 0.380 0.331 0.008  
0 0.313 0.340 0.325 0.340 0.307 0.009  
1 0.281 0.300 0.289 0.300 0.283 0.010 0.227
2 0.266 0.284 0.258 0.284 0.263 0.011 0.219
3 0.250 0.259 0.229 0.259 0.244 0.012 0.212
4 0.234 0.238 0.204 0.238 0.225 0.013 0.207
5 0.219 0.220 0.182 0.220 0.207 0.014 0.204
6 0.203 0.203 0.162 0.203 0.192 0.016 0.201
7 0.188 0.180 0.144 0.180 0.177 0.018 0.199
8 0.179 0.165 0.128 0.165 0.162 0.020 0.197
9 0.156 0.148 0.114 0.148 0.148 0.022 0.194
10 0.141 0.134 0.102 0.134 0.135 0.024 0.191
11 0.125 0.120 0.0907 0.120 0.121 0.026 0.188
12 0.109 0.109 0.0808 0.109 0.106 0.029 0.185
13 0.094 0.095 0.0720 0.095 0.092 0.031 0.182
14 0.078 0.083 0.0641 0.083 0.080 0.033 0.180
15 0.0703 0.072 0.0571 0.072 0.072 0.035 0.178
16 0.0625 0.065 0.0508 0.065 0.063 0.037 0.175
17 0.0563 0.058 0.0453 0.058 0.054 0.039 0.172
18 0.0500 0.049 0.0403 0.049 0.048 0.041 0.168
19 0.0438 0.042 0.0359 0.042 0.041 0.043 0.164
20 0.0375 0.035 0.0320 0.035 0.035 0.045 0.161
21 0.0344 0.032 0.0285 0.032 0.032 0.047 0.157
22 0.0313 0.028 0.0253 0.028 0.029 0.049 0.155
23 0.0281 0.025 0.0226 0.025 0.026 0.051 0.153
24 0.0250 0.022 0.0201 0.022 0.023 0.055 0.151
25 0.0219 0.020 0.0179 0.020 0.020 0.059 0.148
26 0.0188 0.018 0.0159 0.018 0.018 0.063 0.146
27 0.0172 0.016 0.0142 0.016 0.017 0.067 0.143
28 0.0156 0.014 0.0126 0.014 0.016 0.071 0.139
29 0.0141 0.013 0.0113 0.013 0.015 0.075 0.134
30 0.0125 0.012 0.0100 0.012 0.014 0.080 0.127
31 0.0109 0.010 0.0089 0.010 0.013 0.085 0.120
32 0.0106 0.009 0.00795 0.009 0.013 0.090 0.115
33 0.0094 0.008 0.00708 0.008 0.012 0.095 0.112
34 0.0086 0.007 0.00631 0.007 0.010   0.110
35 0.0078 0.005 0.00561 0.005 0.0095   0.108
36 0.0070 0.004 0.005 0.004 0.0090   0.106
37 0.0066   0.00445   0.0085   0.103
38 0.0063   0.00397   0.0080   0.101
39 0.0059   0.00353   0.0075   0.099
40 0.0055   0.00314   0.0070   0.097

Related Topics

  • Miscellaneous

    Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2008). Standard Gauges. [online] Available at: https://www.engineeringtoolbox.com/standard-gauges-d_1345.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.